Thermosetting Silk

KIMONO - Thermosetting Yarn.

63% Silk Shape & 37% Polyester, 2/140 Nm (70.000 Nm).

Final pressing at 170-180oC for one minute to create a stiff body structure. Temperature and timing may vary according to the stitch, weight and the result wanted.

Helpful Hints:

Knit as a 1-ply on 18 gauge flat bed machine. Hand wash recommended.